Nickel Superalloy Rod & Bar Stock

Nickel Superalloy Rod and Bar Stock are essential raw materials for manufacturing components used in the most severe chemical and high-temperature environments. Alloys like Hastelloy C-276 (UNS N10276) are renowned for their universal corrosion resistance, resisting a vast range of media including wet chlorine gas, hypochlorites, and strong oxidizing salts like ferric and cupric chlorides. The high content of Nickel, Molybdenum, and Chromium ensures exceptional resistance to localized attacks like pitting and crevice corrosion. Zeron Fastners supplies certified, high-quality Nickel Superalloy Bar stock in various forms for use in pollution control equipment, chemical processing vessels, heat exchangers, and sour gas applications, guaranteeing component longevity and process reliability.

Related Products

Nickel Superalloy Rod 358

Nickel Superalloy Rod Chemical Composition

Element Composition (%)
Nickel (Ni) Balance (Minimum 50.99)
Molybdenum (Mo) 15.0 to 17.0
Chromium (Cr) 14.5 to 16.5
Iron (Fe) 4.0 to 7.0
Tungsten (W) 3.0 to 4.5
Carbon (C) 0.01 maximum

Nickel Superalloy Rod Mechanical and Corrosion Properties

Property Value (Rod or Bar Minimum)
Ultimate Tensile Strength 758 MPa (110 ksi)
Yield Strength (0.2% Offset) 363 MPa (52.6 ksi)
Corrosion Resistance Exceptional (Reducing and Oxidizing)
Pitting/Crevice Resistance Outstanding
Weldability Excellent (As-welded condition)