Nickel Superalloy Sheet & Plate

Nickel Superalloy Sheet and Plate are essential mill products for fabricating components used in demanding industrial conditions, particularly those involving high temperatures and corrosive chemicals. Alloys like Inconel 600 (UNS N06600) are renowned for their exceptional oxidation resistance at high temperatures, effective defense against carburization, and robust resistance to chloride-ion stress-corrosion cracking. The sheet and plate forms are readily weldable and formable, making them ideal for manufacturing heat treatment furnace muffles, thermocouple sheaths, chemical process equipment, and aerospace components. Zeron Fastners supplies certified, high-quality Nickel Superalloy Sheet and Plate, meeting stringent material specifications for long-term reliability in severe service.

Related Products

Nickel Superalloy Sheet 371

Nickel Superalloy Sheet Chemical Composition

Element Composition
Nickel (Ni) 72.0 minimum
Chromium (Cr) 14.0 to 17.0
Iron (Fe) 6.0 to 10.0
Manganese (Mn) 1.0 maximum
Copper (Cu) 0.50 maximum
Carbon (C) 0.15 maximum

Nickel Superalloy Sheet Mechanical & Thermal Properties

Property Value
Ultimate Tensile Strength 550 MPa
Yield Strength (0.2% Offset) 205 MPa
Max Operating Temperature (Approx.) 1150°C (2100°F)
Oxidation Resistance Excellent
Stress Corrosion Cracking Highly Resistant