Nickel Superalloy Washer

Nickel Superalloy Washers are high-performance load-distributing components manufactured from advanced nickel-based alloys like Inconel 718, Hastelloy C-276, and Monel K500. Zeron Fastners specializes in providing washers that retain their structural integrity and hardness at extremely high temperatures and in severe corrosive environments. The primary function of this product is to ensure consistent load distribution and prevent damage or thermal deformation of the mating surface in critical flanged joints. These washers are essential in aerospace engine mounts, gas turbines, chemical reactors, and high-pressure valves.

Related Products

Nickel Superalloy Washer

Nickel Superalloy Washer Key Grades and Properties

Grade Example Key Property Temperature Resistance Application Highlight
Inconel 718 High Creep-Rupture Strength Up to 700 °C Aerospace, Gas Turbines
Hastelloy C-276 Excellent Pitting & Crevice Corrosion Moderate to High Chemical Processing, Pollution Control

Nickel Superalloy Washer Mechanical Properties (Inconel 718)

Condition Tensile Strength (min) Yield Strength (min)
Solution Annealed 900 MPa 520 MPa
Age Hardened 1240 MPa 1035 MPa